just curious what everyone recommends for welding handbook and or references. im planning on bending and TIGing a cage for my car in the near future out of 4130 and would like to do a little research about the pre and post welding processes, filler material, etc.

thanks javier
Custom Turbo Applications
 
For drag race applications there are standards that address the construction and welding of roll cages. while they closely follow aircraft practices in fitup and joint design the industry standard for 4130 roll cage welds is 70s-2 rod no pre or post heat of joint that is tig only by the way.

The AWS is releasing a new standard that addresses the race car industry`s practices or so ive been told.

For approved tubing O.D. and wall thickness specs. you will need these;

A rule book for the association that the car will run in and this website: