Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Liquid Ring Compressors - MOC

Status
Not open for further replies.

SJones

Petroleum
Joined
Apr 22, 2001
Messages
3,943
Location
GB
Does anyone have experience of operating liquid ring compressors constructed from 316 SS in high H2S (45%) at around the 2 bar WP and 9 bar DP range? If so, would they care to share it on here? Many thanks.

Steve Jones
Materials & Corrosion Engineer
 