hatudi
Mechanical
- Jul 17, 2008
- 10
We are seeing small bulges in the internal liner of a multi-wall reactor vessel. It appears that in the bottom third of the reactor, the liner has pulled away from the wall in several places. We think that this may have been caused by some form of pressure surge. Has any one experienced a similar phenomena?