I was digging through some old weld specs and ran across "Linde 86" called out as a consumable. Is that the same thing as ESAB Spoolarc 86?

Jeff Parham
Mechanical Engineer
Mining Trucks
 
They are both AWS A5.18, class ER70S-6 wires. ESAB lists their wire as "L-TEC/Spoolarc 86" in their data book.
 
My old list(Airco) shows the same classification as posted by dbooker30 but lists Spoolarc 88 instead of Spoolarc 86 under the heading ER70S-6.
 