Limits of the plastic material model

Status
Not open for further replies.

MyNameIsUser

Mechanical
Dec 20, 2013
13
hi, i read the documentation on this but could not get a definite answer out of it (though i believe to have read it somewhere):

For this model to work i need to supply pairs of yield stress/plastic strain points that lead to a stress strain curve that has an decreasing gradient after its elastic section, right? Else it will fail?
 
Replies continue below

Recommended for you

Hi, as you have to input true stress-strain data, and not engineering (or nominal) stress-strain data, the stress and plastic strain values have always to increase each line. E.g.:

400.0, 0.0 (while 400.0 is the yield stress)
410.0, 0.05
415.0, 0.1
...

Otherwise I think Abaqus issues an error message.
 
Hello,

thank you for your answer.
This was not what i was asking:

I asked, whether Abaqus' ordinary plastic material model needs a yield stress/strain table whos graph has a decreasing inclination (as metals usually have in their plastic region)
 