Hello Eveone.

I am looking for references about the behaviour of ASTM A 213 T12.

Does anybody have a Bibliography where I can Find the maximum temperatures for this material, without worring with creep?

Regards.
 
Have you looked in ASME Section II, Part D? Note T5?
 
What do you mean about Note T5???
 
The maximum service temperature for time independent properties for this material is based on ASME Section II, Part D, is 900 deg F.
 
re: NOTE T-5

At the end of Table 1A Ferrous Materials [which your stuff is] there are groups of endnotes:

General Notes (a) thru (f)
NOTES - General Requirements G1 thru G44
NOTES - Heat Treatment Requirements H thru H5
NOTES - Size Requirements S1 thru S9
and the set you need
NOTES - Time-Dependant Properties T1 thru T10

and the last set is NOTES - Welding Requirements W1 thru W15

there are probably more NOTES in some sections now, I'm working from a 2003 book

Lastly, to do ASME Code work, you have to own ASME Code Books. For Sect VIII Div-1 work, that is VIII Div-1 [of course], Sect IX, Sect II-A, -B, -C, and -D, and Sect V. Without those, you are guessing.
 