Dec 3, 2019 #1 siretb Chemical Joined Jul 22, 2003 Messages 198 Location FR Hi Solids, some humidity present in atmosphere .? about 15% huimidy volume% in above atmosphere) Would a blend of clacium chloride (CaCl2,6H2O) 70% wt and lime (Ca(OH)2 30% corrode carbon steel at 70°C
Hi Solids, some humidity present in atmosphere .? about 15% huimidy volume% in above atmosphere) Would a blend of clacium chloride (CaCl2,6H2O) 70% wt and lime (Ca(OH)2 30% corrode carbon steel at 70°C
Dec 5, 2019 #2 cap1a79 Materials Joined Jul 11, 2013 Messages 109 Location US If the level of calcium chloride is 70 %, definitely CS is not suitable while lime water (Calcium hydroxide) is not corrosive. Refer to the below. https://www.materials.sandvik/en/materials-center/corrosion-tables/calcium-chloride/https://www.materials.sandvik/en/materials-center/corrosion-tables/calcium-hydroxide/ If you are looking for the data with calcium chloride with lime (7:3), you need specific test on your own. Although I do not know the details but you may need to consider non-metallic coating. Lee SiHyoung, Upvote 0 Downvote
If the level of calcium chloride is 70 %, definitely CS is not suitable while lime water (Calcium hydroxide) is not corrosive. Refer to the below. https://www.materials.sandvik/en/materials-center/corrosion-tables/calcium-chloride/https://www.materials.sandvik/en/materials-center/corrosion-tables/calcium-hydroxide/ If you are looking for the data with calcium chloride with lime (7:3), you need specific test on your own. Although I do not know the details but you may need to consider non-metallic coating. Lee SiHyoung,
Dec 10, 2019 #3 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,005 Location IN Dear siretb, CS would develop weld cracks around 650C in the said service. Regards. DHURJATI SEN Kolkata, India Upvote 0 Downvote
Dear siretb, CS would develop weld cracks around 650C in the said service. Regards. DHURJATI SEN Kolkata, India
Dec 10, 2019 Thread starter #4 siretb Chemical Joined Jul 22, 2003 Messages 198 Location FR Thank you all. If I understand correctly, the alkalinity of the lime will not mitigate the corrosive potential of calcium chloride Upvote 0 Downvote
Thank you all. If I understand correctly, the alkalinity of the lime will not mitigate the corrosive potential of calcium chloride
Dec 10, 2019 #5 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,005 Location IN Dear siretb, Lime alone is capable of producing those weld cracks in CS. Regards. DHURJATI SEN Kolkata, India Upvote 0 Downvote
Dear siretb, Lime alone is capable of producing those weld cracks in CS. Regards. DHURJATI SEN Kolkata, India
Dec 16, 2019 #6 springrise Civil/Environmental Joined May 1, 2014 Messages 23 Location AT hi, is that a solid powder or a water solution? If a solution, you haven't specified the concentrations. Upvote 0 Downvote
hi, is that a solid powder or a water solution? If a solution, you haven't specified the concentrations.