How often is the test for Lightweight Particles in Aggregates (ASTM C123, AASHTO T 113 or similar) conducted in your area (e.g., daily, weekly, monthly, rarely, never)? Please indicate your geographical location/region.
 
I work in a crushed plant, and we run this test every week.
 