Evidently there is a massive recall for light poles manufactured by Whitco LP and sold in the last ten years. Generally these are poles over 70 feet tall. While there have been some dramatic failures, no one has been hurt - yet. The company is out of business (no surprise) and the schools and towns have no recourse and face costly replacement/repair options.
Apparently the welds seem to be the issue. Do any of you have first hand experience with these poles or the actual cause of the failures? Some of the photos of dismantled poles show large horizontal cracks in the pole-to-base-plate weld.
I am trying to get a sense of whether the failure is due to the design itself or the weld craftsmanship. Some of the articles point to the fact that the pole material may hace come from Mexico, but it is not clear where the base plate fabrication took place.