Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Liebherr Orion crane failure under 5500t load test (II) 1

Status
Not open for further replies.

FacEngrPE

Mechanical
Joined
Feb 9, 2020
Messages
1,666
Location
US
thread815-468694
The original thread is closed. The collapse of the Orion 1 (may 2020) during initial proof testing was a spectacular failure. It has taken Liebherr some time to get repairs organized, but finally they are coming together. This is news of the repairs since the last entry in the original thread.

‘Installation vessel Orion was whiplash proof, but its crane was not’, Published on 17-09-2020 at 09:41

Liebherr Recovers Orion’s Crane Jib, Repair to Be Completed in 2021, November 11, 2020,

It was just announced that Gdańsk Remontowa Shiprepair Yard has contracted to repair the ship.
Gdańsk Remontowa will repair offshore installation vessel Orion I, Published on 02-04-2021

I was not able to find anything more detailed on the hookblock failure.



 