mw87, if the head will take the load applied by the leg, and / or the head and legs are not dissimilar materials, you may be able to omit the pad.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Pad shall be avoided for design temperature <-10ºC or > 450ºC.

Regards
r6155
 