Hi All,
Really need your insights on the problem i'm currently facing for shell and tube heat exchangers.
This is AFS type HX, which having floating tubesheet complete with floating head.
Problem is during Hydrotest, leaking start to occur at this floating tubesheet to floating head joint.
It's only a water drop but consistently happening. tter.
Gasket used for this joint is Kammprofile SS316L. Tubesheet and flange head is Duplex.
We have tried to change the gasket to spiral wound SS316L but the issue resists.
Bolt tightening and torquing has been done according to torque value and in properly sequence.
This unit HT pressure is 65 bar.
Leaking start during building up pressure from 56 bar.
Anyone of you ever experience the similar as above?
I appreciate your advise please.
Really need your insights on the problem i'm currently facing for shell and tube heat exchangers.
This is AFS type HX, which having floating tubesheet complete with floating head.
Problem is during Hydrotest, leaking start to occur at this floating tubesheet to floating head joint.
It's only a water drop but consistently happening. tter.
Gasket used for this joint is Kammprofile SS316L. Tubesheet and flange head is Duplex.
We have tried to change the gasket to spiral wound SS316L but the issue resists.
Bolt tightening and torquing has been done according to torque value and in properly sequence.
This unit HT pressure is 65 bar.
Leaking start during building up pressure from 56 bar.
Anyone of you ever experience the similar as above?