Hello Seniors!
We are repairing a riveted tank which is constructed in 1908. After integrity assessment report generated the scope of work.We have replaced
*All the bottom plates.
*All the roof plates.
*1st shell course.
*300mm width of patch plate on the top shell through out circumference below the curb angle.
Now during hydrotest we encountered several rivets weeping and horizontal lap joints(fillet weld) leakage.We performed seal pass on some rivets and on 2 of the horizontal lap joint through out the circumference.
Now after again refilling some of the rivets started weeping.
Now my client did not want to construct it from zero level(that we suggested before the integrity report).What are the options i have?
Only idea i have is that Patch plates on all the rivet joints from inside and after that painting with some polyurethane mixture on all the patches.
Tank Data Sheet and some leakage photos has been attached.
Thanks in advance.
We are repairing a riveted tank which is constructed in 1908. After integrity assessment report generated the scope of work.We have replaced
*All the bottom plates.
*All the roof plates.
*1st shell course.
*300mm width of patch plate on the top shell through out circumference below the curb angle.
Now during hydrotest we encountered several rivets weeping and horizontal lap joints(fillet weld) leakage.We performed seal pass on some rivets and on 2 of the horizontal lap joint through out the circumference.
Now after again refilling some of the rivets started weeping.
Now my client did not want to construct it from zero level(that we suggested before the integrity report).What are the options i have?
Only idea i have is that Patch plates on all the rivet joints from inside and after that painting with some polyurethane mixture on all the patches.
Tank Data Sheet and some leakage photos has been attached.