If I were to redesign a light truck's rear suspension I would like to reduce the compliance oversteer.
It seems to me that one thing that would help would be to put the hanger at the front of the leaf spring.
Has anyone tried that? What problems did it cause?
I realise it would tend to cause more driveline plunge, and ground clearance might be an issue, but other than that I can't see a downside.
Alternatively, other than fitting a Panhard rod, has anybody got any neat suggestions to get the same effect?
Cheers
Greg Locock
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips.
It seems to me that one thing that would help would be to put the hanger at the front of the leaf spring.
Has anyone tried that? What problems did it cause?
I realise it would tend to cause more driveline plunge, and ground clearance might be an issue, but other than that I can't see a downside.
Alternatively, other than fitting a Panhard rod, has anybody got any neat suggestions to get the same effect?
Cheers
Greg Locock
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips.