Jul 21, 2004 #1 bicolexpress Mechanical Joined Jun 24, 2003 Messages 29 Location PH Good day, somebody out there help me find the viscosity of lead at 650deg.C thanks
Jul 21, 2004 1 #2 TD2K Chemical Joined Jan 11, 2002 Messages 2,629 Location US 551C = 1.70 cP 600C = 1.38 cP 703C = 1.349 cP 844C = 1.185 cP Handbook of Chemistry and Physics, 60th edition. Upvote 0 Downvote
551C = 1.70 cP 600C = 1.38 cP 703C = 1.349 cP 844C = 1.185 cP Handbook of Chemistry and Physics, 60th edition.
Jul 29, 2004 Thread starter #3 bicolexpress Mechanical Joined Jun 24, 2003 Messages 29 Location PH TD2K, THANKS A LOT. Upvote 0 Downvote