somebody out there help me find the viscosity of lead at 650deg.C
thanks
 
Replies continue below

Recommended for you

551C = 1.70 cP
600C = 1.38 cP
703C = 1.349 cP
844C = 1.185 cP

Handbook of Chemistry and Physics, 60th edition.
 