Does anyone know if it is possible to plate 316L st/st
with high puriy lead.
Any help greatly appreciated.
 
Replies continue below

Recommended for you

I have seen Tern plated stainless used for roofing. So I suppose that high purity lead is possible. You may need a bond layer of Cu or Ni though to get a good surface.

= = = = = = = = = = = = = = = = = = = =