Chapter 5, Volume 3, 8th Edition of the AWS Welding Handbook provides much info on lead welding, wiping and soldering. The last time, that I was associated with lead pipe welding was 30 years ago and it was difficult to find capable welders/burners then - no "lead pipe cinch". Today, I suspect, it is nearly a lost art. Wish you the best of luck.