I need to use steel able to resist sour gas attack and I am familiar with the idea of normalizing the (Carbon) steel grain size and controlling the material and weld hardness to minimize the risk of intergranular attack.
"Tempering" was recently thrown around in a discussion and I'm a little confused. Doesn't this harden the surface again or am I off-base?