I need to laser weld a 304L disk (dia.480x .001"thk) to an opening in a 17-4PH body to create a sealed port. I am not familiar with laser welding at all (new industry for me). Do I have to worry about warping or other positional issues such as work holding?.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
You should consult with the welder how to machine and prepare the opening such that it will fix the disc in place. I am not sure that the 0.001" is not too thin for laser weld but I think that the Micro TIG can do it.
 
Sorry, that was a typo, it should be .011"thk. The disk fits into a counterbored area like a spotface. I had originally thought TIG as well, but was told to laser weld it.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
I meant Micro TIG not TIG. A company I worked for ordered custom design miniature sealed bellow (~1/2" dia) made by Micro TIG of many beveled disks ~0.1-0.2 mm thick.
 
We used laser welding to weld the bellow to a solid tube.
 