We have a job that requires us to cut stainless steel with pvc coating on one side. the application requires that we leave the pvc coating on the material. we have attempted to score the pvc with low wattage and a raised focal point and then cut the stainless. The coating blows off when we attempt to pierce and cut the material. We have tried nitrogen as the assist gas at a range of pressures (125psi-200psi) and the film still blows off. We also tried oxygen cutting the material at 20 psi and the film still blows off. Does anyone have experience with a similar application that could offer some guidance?