Are most laser beam welding procedure qualifications done in accordance with AWS C7.4 or AWS D17.1?
 
Replies continue below

Recommended for you

I would venture to say C7.4 rather than D17.1. There are many automotive and general industrial applications that would never reference D17.1.
 