Nov 11, 2013 #1 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US Are most laser beam welding procedure qualifications done in accordance with AWS C7.4 or AWS D17.1?
Nov 11, 2013 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US I would venture to say C7.4 rather than D17.1. There are many automotive and general industrial applications that would never reference D17.1. Upvote 0 Downvote