I recently visited a single-family house with multiple wide cracks in the concrete basement wall. It's quite old and no reinforcement is visible. The client shared that they have minimal water intrusion through the cracks and I can see why that is. There's an 8-foot addition beyond the basement wall that cause the water to run away from it for the most part. I doubt if there are any immediate structural concerns and don't think any remedies beyond proper sealing of the cracks are necessary. But my question is what could have possibly caused such cracks. There are no signs of settlement or any other cracks in the floors above. Any thoughts? I've included a picture.