Feb 5, 2009 #1 leslie2000 Materials Joined Jun 11, 2008 Messages 22 Location JP Hi, anyone knows whether it is possible to produce 15x105x150mm Sm2Co17 blocks? Magnetized through 150mm direcction.
Hi, anyone knows whether it is possible to produce 15x105x150mm Sm2Co17 blocks? Magnetized through 150mm direcction.
Feb 5, 2009 #2 MagMike Materials Joined Jun 4, 2003 Messages 506 Location US Not as one solid piece. It'll have to be built up from smaller pieces. Upvote 0 Downvote
Feb 5, 2009 Thread starter #3 leslie2000 Materials Joined Jun 11, 2008 Messages 22 Location JP Thanks MagMike, do you know if there is difference in magnetic performance if we build up with several smaller pieces? Upvote 0 Downvote
Thanks MagMike, do you know if there is difference in magnetic performance if we build up with several smaller pieces?
Feb 6, 2009 #4 MagMike Materials Joined Jun 4, 2003 Messages 506 Location US No, there is no significant difference. Upvote 0 Downvote