Dear All,
As per API 650 ed 12 2016, para 5.1.3.5 Lap-welded joints, as tack-welded, shall be lapped as follows: - Single-welded joints shall be lapped at least five times the nominal thickness of the thinner plate joined, or 25 mm (1 in.), whichever is smaller.
From the statement above, is it right if we lap:
1. bottom plate to bottom plate by minimum 25 mm?
2. bottom plate to annular bottom plate by minimum 25 mm?
Help me with this, as I could not find a specific statement that rules the lap between bottom to bottom plate or bottom to annular plate.
Thanks for the help!!!
As per API 650 ed 12 2016, para 5.1.3.5 Lap-welded joints, as tack-welded, shall be lapped as follows: - Single-welded joints shall be lapped at least five times the nominal thickness of the thinner plate joined, or 25 mm (1 in.), whichever is smaller.
From the statement above, is it right if we lap:
1. bottom plate to bottom plate by minimum 25 mm?
2. bottom plate to annular bottom plate by minimum 25 mm?
Help me with this, as I could not find a specific statement that rules the lap between bottom to bottom plate or bottom to annular plate.
Thanks for the help!!!