Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Laboratory test on mechanical couplers

Status
Not open for further replies.

ABA102

Structural
Mar 3, 2017
59
Hi,

I'm in a project where the Specs. required 3 lab. tests on mechanical couplers, can anyone share me a clause in a code stating what are the 3 tests required for mechanical couplers except for tension test?

 
Replies continue below

Recommended for you

Eurocode 8 is seismic, which place load reversal demands on couplers. Fatigue can also be an issue, in some circumstances.

ISO 15835-2:2018 Steels for the reinforcement of concrete — Reinforcement couplers for mechanical splices of bars — Part 2: Test methods might be a good place to start.
 
One tension test, performed three times?
Have you reached out to the person who wrote the spec?
 
I agree, ask the spec writer. Maybe the intent is 3 slip tests.IS there any other info in the spec? In coupler/connector specs that I'm familiar with, slip is the only test I've seen specified (for bridge work that's generally good enough). ASTM A1034 describes six types of tests, including slip.
 