I have a spot for label on this product that has a operating temp around 100C
I don't want the label to by itself peel out or deform due to temp.
There is no way to open the product in field to replace labels.

So I request suggestion on label material or any special stick on labels

Thx
C1
 
Replies continue below

Recommended for you

Engraved or laser etched on stainless steel, attached with rivets.
 
Many polyester labels have a 150deg C max service temperature..
 
What is the material of the part?
Can the part itself be engraved or silk screened?
 
Part is AL1100. I think I like the idea of engraving. Thx guys.
 
If you anodize and dye the aluminum, you can "etch" (more like bleach) the dye with a CO2 marking laser, leaving a silver mark where the laser hits, with good contrast to the (hopefully) contrasting anodized surface.
 