jamesframes
Mechanical
I am evaluating mag drive centrifugal pumps for circulating hot KOH (typically 20-45% at ambient to 195F). Flow is thru a filter/strainer and then an in-line heater. Flow rate to be around 4-6 gpm. Submerged suction.
I have to eliminate PP pump bodies becuase of the high temperature and can't use PVDF becuase of the high Ph. That leaves me with 316SS (or ECTFE which is uncommon).
I believe carbon bushings will be OK - as well as silicon-carbide.
I would appreciate any thoughts or suggestions? Also, is there a good way in this case to provide dry running protection?
I have to eliminate PP pump bodies becuase of the high temperature and can't use PVDF becuase of the high Ph. That leaves me with 316SS (or ECTFE which is uncommon).
I believe carbon bushings will be OK - as well as silicon-carbide.
I would appreciate any thoughts or suggestions? Also, is there a good way in this case to provide dry running protection?