We are trying to make a composite surface that we can clamp a 2.0-mm wire onto that will be required to carry a transverse load. We are having problems making the surface of our composite hard enough to prohibit the wire from sinking into the surface when we clamp down on it. Does anyone know if a layer of Kevlar will provide us with this increased hardness and what thickness we should use? Or is there some other way that we can increase the surface hardness of our composite we've tried several mesh angles and temperature ranges but with very little success.