I own land near Sparta, georgia that has been tested for Kaolin and the company that has been testing has found one million tons of raw product that they want to mine. I currently have a contract that my father negotiated for $1.50 per ton of raw product and the company wants to renegotiate the contract to lower the price to $.55 cents per ton.
How can I talk to an expert that can advise me as to what the current price should be? I would really appreciate some help!
Thanks!
I own land near Sparta, georgia that has been tested for Kaolin and the company that has been testing has found one million tons of raw product that they want to mine. I currently have a contract that my father negotiated for $1.50 per ton of raw product and the company wants to renegotiate the contract to lower the price to $.55 cents per ton.