Can anyone recommend a potting compound for an electronic circuit card that could withstand JP10 fuel vapour for 30 days without significant swelling or degradation ?

Thanks

Nick Stilwell
 
Replies continue below

Recommended for you

How about PR1422 fuel tank sealant. I'v enver used it on electronics but I suspect it would be OK - worth a try.
 
Try to look at BMS8-68D. This is also found by part number CS3808 and is multi part kit. Boeing uses this potting compound on electrical connectors for fuel qty system and is in JP-8. I don't know if it is compatible with MIL-P-87107, but chances are good?
 