I'm trying to determine the coating on a stainless steel (316) joint. It is white and easily scraped off with a coin. Air is it the pipeline at about 10 bar 200 deg C.

Any help is appreciated.

allan
 
Replies continue below

Recommended for you

MOM?

(really thats what I've heard makes an awesome antisieze.)

other than that I'd figure on one of the commercial pipedopes.
 
If the pipe is several years old it might be "White Lead". The standard pipe dope for many years and still shows up on ocassion.
 