Hi,
I want to make a joint between:
a: metal plate thicknes: 5 mm to a hollow section 50x50x3.2
b) metal plate thickness: 5mm to a metal plate 12 mm thickness.
what is the size of the bolt that suits these joint or should I weld it? tq.
 
There's not enough information provided to give you a proper answer.

What loads/forces are involved?
What dynamics are at play with the joint?
Ect, ect.

MadMango
"Probable impossibilities are to be preferred to improbable possibilities."
Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top