Joining 2 pieces of Nickel Plated Stainless Steel together

Status
Not open for further replies.

realphx

Computer
Joined
Oct 11, 2010
Messages
1
Location
US
I have two parts... a magnet and a threaded base. They are both Nickel Plated Stainless Steel. I would like to connect them together.

What would the best method be?
Glue? Solder?

By the way I am not an engineer I'm just asking the professionals.
 
solder would be my vote,

Try a super glue, i dont know what kind of stressess it will endure though.
 
What is the maximum temperature the magnet can withstand before being damaged / losing magnetic properties? If the magnet can withstand heat then a silver solder or braze may be an option. An epoxy optimised for nickel - an awkward metal to bond IIRC - might be an option too.


----------------------------------
image.php

If we learn from our mistakes I'm getting a great education!
 
Please provide photographs of the objects.



Mike Halloran
Pembroke Pines, FL, USA
 