Does material JISG3131-SPHC and ASTM A36 are equivalent?
Here, equivalent is limited to mechanical properties, chemical composition and others testing requirements not for Code or Standard judgment
 
Replies continue below

Recommended for you

For your intentions, you need to obtain a copy of the JIS G3131 and compare to a copy of ASTM A 36.
 
meterng,

I have tried to compare both of them, but I can't find both are "typical" material based on chem analysis & mech properties. There some properties different to much.
Can you help me to determined both are "equivalent"
 
 http://files.engineering.com/getfile.aspx?folder=dbd21e5a-d8b3-4909-a45a-152102a002e7&file=Compare_A36_vs_JIS_SS400.pdf
dursosono;
What is the application where you want to substitute the A36 for G3131? The attachment you provided is not complete with the necessary information.
 
If your inquiry is for API-650 tank construction, please refer to Section 4.2.5 and Table 4-2. Your answer lies there.