I'm looking at extending a jib crane support by 18" and plan to use an HSS 16"x0.375 tube with 1" plates welded top and bottom with holes to match existing bolt circle. Does anyone have a handi-dandi formula for checking the a tube with fixed ends for flexural stability, so no elastic buckling? Thanks in advance.

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
Hi dik

Any chance of a sketch to see exactly what you intend?

“Do not worry about your problems with mathematics, I assure you mine are far greater.” Albert Einstein
 
Something Like...
image_p6qaqz.png


Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
I would use something like that for combined loads on stacks or vertical vessels. References would be ASME STS-1 CL 4.4.1 & 4.4.2 or ASME VIII-2 Part 4.4.12. Otherwise, any pressure vessel design manual will have methods for design of skirt supports and combined loadings on vertical vessels.
 

Hi DIK,

For this case, LTB is not critical.. You are expected to check for bending , shear , torsion etc..

You may look API RECOMMENDED PRACTICE 2A-WSD (RP 2A-WSD) for the allowable stresses for the cylindrical members.

 
 https://files.engineering.com/getfile.aspx?folder=d336cf3c-4810-46ea-a1dd-0f209316a3c3&file=API_ALLOWABLE_STRESSES_FOR_CYLINDRICAL_MEMBERS.pdf
Roark's :
1 - ch 12 formulas for short columns + table 12.1

2 - ch 13 shells of revolution, pressure vessels + table 13.1
 
Thanks...

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
dik..

I believe that it would be reasonable for you to post your final calculations on this thread

Completion and distribution of your work would help others and enrich eng-tips in the long run

Best Regards

MJC

MJCronin
Sr. Process Engineer
 
@hturkak: Based on your API reference, I found an equivalent ISO document in LRFD... thanks, again.

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 