Apr 6, 2020 #1 MElsayd Mechanical Joined Jul 6, 2019 Messages 2 Location QA Good evening Gents, Would you advise me please Why jet Fuel line isn't required lining
Apr 6, 2020 #2 MJCronin Mechanical Joined Apr 9, 2001 Messages 5,102 Location US Why do you feel that Jet Fuel piping requires lining ? Jet fuel is a refined hydrocarbon, like gasoline and diesel fuel .... Do you feel that they also require lining ??? MJCronin Sr. Process Engineer Upvote 0 Downvote
Why do you feel that Jet Fuel piping requires lining ? Jet fuel is a refined hydrocarbon, like gasoline and diesel fuel .... Do you feel that they also require lining ??? MJCronin Sr. Process Engineer
Apr 7, 2020 #3 SJones Petroleum Joined Apr 22, 2001 Messages 3,943 Location GB The usual thinking behind lining is to prevent contamination from corrosion products. If this isn't a concern, there may not be need to line. Perhaps give us some more to work with. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
The usual thinking behind lining is to prevent contamination from corrosion products. If this isn't a concern, there may not be need to line. Perhaps give us some more to work with. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer.