What stainless steels can be used in a high tensile strength condition immersed in jet fuel?

(high tensile strength means UTS>200ksi)

nick

Nick
I love materials science!
 
Consider 17-4 PH, Inconel 718 or posibly A286 or Nitronic 40,50,60 (Cold worked).
 
Ok so will 17-7 work or is there something in the extra nickel that causes a problem?

nick
 