Is there a product similar to flexcell that is placed between a concrete structure and new asphalt pavement?

Dik
 
I agree with SRE that the flexible material between concrete and asphalt is normally....asphalt.
 
Thanks... its the cold climate I was concerned about.

Dik
 
How about some sort of bond break like felt paper?
 
I went out last night to see what the city does with asphalt to concrete curb and they don't do anything. I think I will avoid a bond breaker and make sure the curb has a tack coat below the asphalt layer (I should have left the typo... I was using a tack cat.)

Dik
 
Attack cat? Like the time I had to take our Sammy to the vet?

NYSDOT is specifying hot melt asphalt joint adhesive at top course cold joints, including curb. Upstate NY certainly counts as cold climate.
 
Typically we just tack coat for asphalt to concrete interface (curb and gutter, concrete pads, etc.).
Unless for airports, they require a routed joint (after paving) with joint sealer between the two.
 
Thanks gentlemen...

Dik
 
dik...just prime the concrete before asphalt placement. If you transition from asphalt to concrete in the traffic lane slope the concrete at 15-20 degrees off vertical so when traffic rolls over it pushes the asphalt against the concrete
 
Thanks, Ron... that's what I did... not usually involved with asphalt... but had to repair some roadway that was cut out for access to a concrete wall. Used 4" HL3 over 12" Cmpt Gran 'A'. Should be good for small trucks and passenger vehicles.