Why is that HIC testing not a requirement for ISO 7778 Z30 plates.
 
Not a requirement of whom, or what document?

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
It so states in a middle east Oil company spec. I was thinking that someone with experience of using the ISO specification plate would know why. I see that HIC testing is a requirement for flat rolled products as plates because of Sulphide inclusions in the material structure interstices.
 
Some companies have a belief that the manufacturing process applied to plate to achieve Z grade properties also provides resistance to HIC that does not need confirmation by HIC testing.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Nice answer, Mr. Jones. [wink]
 
Can you think of the relevance of the through thickness properties and resistance to HI cracking?
 
Sulphide shape control in steel making would be the first thing that springs to mind: it would have an effect on both properties.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 