Does level 2 apply for range qualified for welders? Please see bellow.

Screenshot_1-4-2024_14224__edaptb.jpg


Screenshot_1-4-2024_14333__lc9mji.jpg
 
Replies continue below

Recommended for you

15614 is for WPQR (welding procedure qualification), not WPQ (welder performance qualification)
 