have a customer that references one standard that references AWS D1.1, then says, but he wants to use AWS D1.6.
i understand the use of D1.6 for SS, but the base standard does not reference it, only D1.1.
i initially burped on his switching criteria not found in the original base reference standard. did i get heartburn over nothing?
i understand the use of D1.6 for SS, but the base standard does not reference it, only D1.1.