Dear All,
I had Radiography Test (RT) for several weld joints and found few are rejected due to porosity. Our Client is insisiting to have more test (we have 5% of the joints) as a penalty of the failure. Is there any penalty on failure of weld joint.
Regards
MAK72
 
Replies continue below

Recommended for you

most times i have seen 10% and if 10% of those get rejected then you do another 10%, if you get another 10% reject then it goes to full RT of welds.
 
sounds about right, depends on which spec, some call for 2 welds extra from welders who made repairs.

need a spec to confirm
 
Standard practice in my industry and very sensible precaution.
1- Set testing frequency
2- No problems, reduced frequency can be considered
3- Problems detected, increase frequency, sometimes as much as 100% until problems disappear.
 
Statistics would say that if you have a representative sample of 10% of the population, the percent failed welds can be extrapolated to the population. So if 10% of the 10% are bad then you can be confident that something like 10% of all the welds are bad, rarely an acceptable outcome on a job where you are bothering to test.

Like the other posters, I would look at the data and any welder with a failed weld would get 20% X-Ray the next day. If ANY of those welds fail I would do 100% of that guy's welds until you get around to running him off.

David
 
Another comment.

Welders hate to repair welds. We always make sure that the welder that had the weld failed is the one repairing it. It goes a long way to make sure he improves.

 
I agree with Zdas04 on that. I've seen many welders go home. I've let them retest a week later or so and let them back to work after some time out.
 