I was told to search for an extruded tube/pipe with an 8" dia. Is there a standard size for the ID or OD? I know it depends on the thickness, but is there a chart to view anywhere?

Thanks
 
Replies continue below

Recommended for you

You probably need to look at DOM (drawn over mandrel) pipe. Any steel supplier should have literature with available sizes.
 
What material is required? Are you looking for pipe or tube, or is only the OD important? What application? Help us to help you.
 