Hi All,
I'm just looking at equation 9 in API 10B-2 (see screenshot below).
And to me it seems like they have made a mistake. I think they should have
slurry_density (lb/gal) = [highlight #FCE94F](1 / 0.1337)[/highlight] * slurry_mass (lb/sack) / slurry_volume (ft^3/sack)
instead of the
slurry_density (lb/gal) = [highlight #FCE94F]0.1337[/highlight] * slurry_mass (lb/sack) / slurry_volume (ft^3/sack)
stated. Does anyone else agree?
I'm just looking at equation 9 in API 10B-2 (see screenshot below).

And to me it seems like they have made a mistake. I think they should have
slurry_density (lb/gal) = [highlight #FCE94F](1 / 0.1337)[/highlight] * slurry_mass (lb/sack) / slurry_volume (ft^3/sack)
instead of the
slurry_density (lb/gal) = [highlight #FCE94F]0.1337[/highlight] * slurry_mass (lb/sack) / slurry_volume (ft^3/sack)
stated. Does anyone else agree?