Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is there a connection like UW-13 for direct connection of Body flange to spherical heads? 3

Status
Not open for further replies.

gh61

Mechanical
Joined
May 25, 2016
Messages
15
Location
DE
Is there a connection like UW-13 for direct connection of Body flange to spherical heads?
 
drawing, dimensions, more details ....?
Regards
 
drawing, dimensions, more details ....?
Regards
Hi
Similar to the attached details
 

Attachments

  • Capture.JPG
    Capture.JPG
    14.2 KB · Views: 23
YES.

Regards
 
OP,
Look up Fig 1-6.
 
Figure 1.6 does not apply.
The OP diagram is a welding neck flange.

Regards
 
VIII-1 UW-13 (b)
(b) See below:
(1) Ellipsoidal, torispherical, and other types of
formed heads shall be attached to the shell with a butt
weld, or as illustrated in the applicable Figure UW-13.1
sketches (a), (b), (c), (d), and (i)

So flanged shell to head connection may not be permissible.
 
@ goutam

You are confused. This is a category A welded joint.

Regards
 
@ goutam

You are confused. This is a category A welded joint.

Regards
Can you explain more?
 
See UW
 
@r6165

Thank you for the info. Actually, it should be a type C joint. But I never handled such a joint.

@gh61

Please see the following from Mandatory Appendix 2(Flanges), Fig 2-4
1731651103246.png
 
This is the type of welding I am referring to:
1731669450411.png

Which clause you are referring to?
 
Again NO
Why don't you read the text and not the sketch?
 
OK I give up as you are not explaining yourself.
 
See also figure UW-3 on the left, the spherical head.
Try to understand about spherical head.
 
It is a flanged connection. So it should be type C as in the figure. Type A is welded connection. This is my understanding.
 
See my sketch

Category A weld joint.jpg
 
Please see VIII-1 MA1 Fig 1.6 for permissible types of bolted dished cover joints.

Please ignore Mandatory Appendix 2(Flanges), Fig 2-4 shown above as it is for bolted piping joints (apologies).
 
Once more you are wrong

IT SEEMS IMPOSSIBLE for you to understand what the OP says in his NOV 2 sketch: the body flange is a WELDING NECK, it is full penetration butt weld !
 