Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is the allowable stress of SA-516 70N same as SA-516 70? 1

Status
Not open for further replies.

ChinaZh

Mechanical
Joined
Oct 2, 2006
Messages
25
Location
US
Dear everyone,

I could not find the allowable stress in ASME Sec II Part D for SA-516 70N. Does that mean that their stresses are the same?

Thank you.
 
Yes. Grade 70 steel under ASME SA-516 must meet the minimum mechanical property requirements, hot rolled or normalized.

See thread330-75119
 