Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Is S 275 JR suitable to be used as Construction Material for Pressure Vessel with steam as a medium?

Status
Not open for further replies.

AAA89

Mechanical
Joined
May 5, 2021
Messages
4
Location
MY
Hi,

I would like to know whether material S 275 JR is suitable to be used as construction material for Unfired Pressure Vessel with steam as a medium? For main pressure part like Shell and Head.

I heard somewhere that there is an incident related to material S 275 JR used as a construction material for steam pressure vessel. No detail explanation regarding on that incident that I can found on the internet. Maybe you guys had heard about it somewhere?.

Thanks
 
Hi,

From what I found, the equivalent ASME spec. is ASME SA-1011 which can't be used as construction material for ASME (U-Stamped) pressure vessels
 
HI IdanPV,

May I know exactly where I can refer regarding on ASME SA-1011 can't be used as construction material? Thank you in advance for your reply
 
Per ASME SECTION VIII Division 1 UCS-5(a):
"All carbon and low alloy steel material subject to stress due to pressure shall conform to one of the Specifications given in Section II and shall be limited to those listed in Table UCS-23"
 
What design code do you apply?

In general I'd say that any S-material, for EN design codes, cant be used for pressure applications. S-materials, in contrast to P-materials, dont have guaranteed material characteristics (like yield and tensile) at elevated temperature. So if you need a pressure vessel material in a 275 grade, use P275 or something similar (afaik, P275 doesnt exist, so youll likely end up with P285 or P235).
Some EN materials are listed for use under VIII-1, as IdanPV mentioned refer to the applicable code section.

Huub
- You never get what you expect, you only get what you inspect.
 
Hi XL83NL,

I used ASME code. Usually we refer to Material Comparison Table for non-ASME material if to be used for construction. However S275JR usually will be compare to SA-36 but only can be used for non pressure part or pressure part only if the medium of the vessel is other than steam.

But as IdanPV stated that if S275JR to be equivalent to SA-1011, then it cannot be used for construction per stated in ASME code.
 
SA-36 is a general specification for carbon structural steels.
SA-1011 is a specific specification for hot-rolled sheets.

 
In one country the usage of EN10025 S275JR for PV pressure part is already forbidden. I have seen a steam service pressure vessel build using JISG3101 SS400 that already in service for 30++ years and still working fine.
 