Is QQZ-325C obsolete?? 1

Status
Not open for further replies.

rubepierre

Industrial
Dec 15, 2001
30
Is it,or is it just less stringent in acid testing?
thank you in advance...rube
 
Replies continue below

Recommended for you

QQ-Z-325C ZINC COATING, ELECTRODEPOSITED was cancelled March 9, 1982, and superseded by ASTM B633.

Please explain further what you mean by acid testing.
 